Mechanical Properties Metric English Comments
Tensile Stress 115.46 MPa

@Strain 0.710 %,
Temperature 0.000 °C
16746 psi

@Strain 0.710 %,
Temperature 32.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G50HSLA BK039B Nylon 66  (Unverified Data**)
50% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers
Tensile Stress 115.46 MPa

@Strain 0.970 %,
Temperature -20.0 °C
16746 psi

@Strain 0.970 %,
Temperature -4.00 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G35HSL NC010 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL NC010 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..