Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.793 MPa @Strain 100 % |
115 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3932C TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 0.790 MPa @Strain 0.230 %, Temperature -40.0 °C |
115 psi @Strain 0.230 %, Temperature -40.0 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |