Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 77.78 MPa @Strain 7.12 %, Temperature 0.000 °C |
11280 psi @Strain 7.12 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It.. |
|||
Tensile Stress | 77.78 MPa @Strain 7.12 %, Temperature 0.000 °C |
11280 psi @Strain 7.12 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati.. |
|||
Tensile Stress | 77.76 MPa @Strain 0.830 %, Temperature 23.0 °C |
11280 psi @Strain 0.830 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® RE5329 BK503 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Glass Reinforced Polyethylene TerephthalateInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 77.78 MPa @Strain 0.700 %, Temperature 23.0 °C |
11280 psi @Strain 0.700 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6
(Unverified Data**) 40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 77.78 MPa @Strain 2.25 %, Temperature 90.0 °C |
11280 psi @Strain 2.25 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G45L NC010 Nylon 6
(Unverified Data**) 45% Glass Reinforced Polyamide 6Zytel 73G45L NC010 is a 45% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |