Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 110.48 MPa @Strain 1.20 %, Temperature 23.0 °C |
16024 psi @Strain 1.20 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT) 30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol.. |
|||
Tensile Stress | 110.48 MPa @Strain 1.20 %, Temperature 23.0 °C |
16024 psi @Strain 1.20 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo.. |