Mechanical Properties Metric English Comments
Tensile Stress 11.7 MPa

@Strain 3.92 %,
Temperature 90.0 °C
1700 psi

@Strain 3.92 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F20 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provi..
Tensile Stress 11.7 MPa

@Strain 3.92 %,
Temperature 90.0 °C
1700 psi

@Strain 3.92 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F20UV WT660 Polybutylene Terephthalate (PBT)
Unreinforced UV Stabilized Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provided..
Tensile Stress 11.7 MPa

@Strain 58.83 %,
Temperature 120 °C
1700 psi

@Strain 58.83 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET  (Unverified Data**)
82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 11.7 MPa

@Strain 0.880 %,
Temperature 90.0 °C
1700 psi

@Strain 0.880 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® FR70M30V0 NC010 Nylon 66  (Unverified Data**)
30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 NC010 is a 30% mineral reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performa..
Tensile Stress 11.7 MPa

@Strain 10.0 %
1700 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc..