Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 11.2 MPa @Strain 0.290 %, Temperature 23.0 °C |
1620 psi @Strain 0.290 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 11.2 MPa @Strain 50.0 % |
1620 psi @Strain 50.0 % |
ISO 527-1/-2 |
DSM Arnitel® EB464-01 TPC-ET Antisqueak Blow Molding Grade |
|||
Tensile Stress | 11.2 MPa @Strain 0.380 %, Temperature 23.0 °C |
1620 psi @Strain 0.380 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers |