Polymer Property : Tensile Stress = 11.02 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 11.02 MPa

@Strain 0.100 %,
Temperature 60.0 °C
1598 psi

@Strain 0.100 %,
Temperature 140 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon  (Unverified Data**)
Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood..
Tensile Stress 11.02 MPa

@Strain 0.180 %,
Temperature 150 °C
1598 psi

@Strain 0.180 %,
Temperature 302 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon  (Unverified Data**)
Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood..