Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 100.54 MPa @Strain 1.30 %, Temperature 40.0 °C |
14582 psi @Strain 1.30 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G50HSLA BK039B Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |