Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 100.39 MPa @Strain 7.07 %, Temperature 90.0 °C |
14560 psi @Strain 7.07 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6