Polymer Property : Tensile Stress = 1.69 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 1.69 MPa

@Strain 100 %
245 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® C4850 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 1.69 MPa

@Strain 100 %
245 psi

@Strain 100 %
ASTM D412
Teknor Apex Monprene® MP-2815A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 1.69 MPa

@Strain 0.150 %,
Temperature 40.0 °C
245 psi

@Strain 0.150 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo..
Tensile Stress 1.69 MPa

@Strain 6.20 %,
Temperature 100 °C
245 psi

@Strain 6.20 %,
Temperature 212 °F
ISO 527
DuPont Performance Polymers Hytrel® G4078W TPC-ET  (Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..