Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.37 MPa @Strain 300 % |
199 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® C4830 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Stress | 1.37 MPa @Strain 100 % |
199 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P1850 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 1.37 MPa @Strain 100 % |
199 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3845H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | >= 1.37 MPa @Strain 100 % |
>= 199 psi @Strain 100 % |
ASTM D412 Method A |
Seals Eastern 7042U Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |
|||
Tensile Stress | 1.37 MPa @Strain 5.71 %, Temperature 0.000 °C |
199 psi @Strain 5.71 %, Temperature 32.0 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b.. |
|||
Tensile Stress | 1.37 MPa @Strain 67.2 %, Temperature 120 °C |
199 psi @Strain 67.2 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b.. |
|||
Tensile Stress | 1.37 MPa @Strain 0.0500 %, Temperature -20.0 °C |
199 psi @Strain 0.0500 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)
(Unverified Data**) Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also.. |
|||
Tensile Stress | 1.37 MPa @Strain 5.71 %, Temperature 0.000 °C |
199 psi @Strain 5.71 %, Temperature 32.0 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 1.37 MPa @Strain 67.2 %, Temperature 120 °C |
199 psi @Strain 67.2 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 1.37 MPa @Strain 0.230 %, Temperature -40.0 °C |
199 psi @Strain 0.230 %, Temperature -40.0 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |