Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.930 MPa @Strain 0.0200 %, Temperature 0.000 °C |
135 psi @Strain 0.0200 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010 UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight... |