Mechanical Properties Metric English Comments
Tensile Stress 0.660 MPa

@Strain 300 %
95.7 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® C4920 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 0.660 MPa

@Strain 0.220 %,
Temperature 0.000 °C
95.7 psi

@Strain 0.220 %,
Temperature 32.0 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers