Polymer Property : Dart Drop Total Energy = 60.1 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Total Energy 60.1 J/cm

@Temperature 23.0 °C
0.113 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion 87560 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Dart Drop Total Energy 60.1 J/cm

@Temperature 23.0 °C
0.113 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion L0148 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: Finished part testing is required for ASTM E-84 certification. Note: The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by Po..
Dart Drop Total Energy 60.1 J/cm

@Temperature 23.0 °C
0.113 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion L9620 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Dart Drop Total Energy 60.1 J/cm

@Temperature 23.0 °C
0.113 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Dry Blend E7506 Polyvinyl Chloride, Rigid (PVC, Rigid)
Geon E7506 is recommended for whites and light pastel colors only. Performs well in extrusion blow molding and high rate fencing capstock applications.Physical properties based on Geon E7506 white 1..