Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 57.8 J/cm @Temperature 23.0 °C |
0.108 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Rigid Extrusion 87775 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Dart Drop Total Energy | 57.8 J/cm @Temperature 23.0 °C |
0.108 ft-lb/mil @Temperature 73.4 °F |
Procedure B, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Rigid Extrusion 87775 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Dart Drop Total Energy | 57.8 J/cm @Temperature 23.0 °C |
0.108 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
PolyOne Geon™ HTX L1502 Polyvinyl Chloride Alloy (PVC Alloy) Physical properties based on Geon HTX L1502 white 1000.Information provided by PolyOne |
|||
Dart Drop Total Energy | 57.8 J/cm @Temperature 23.0 °C |
0.108 ft-lb/mil @Temperature 73.4 °F |
Procedure B, C.125; ASTM D4226 |
PolyOne Geon™ HTX L1502 Polyvinyl Chloride Alloy (PVC Alloy) Physical properties based on Geon HTX L1502 white 1000.Information provided by PolyOne |
|||
Dart Drop Total Energy | 57.8 J/cm @Temperature 23.0 °C |
0.108 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Dry Blend E6950 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |