Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 57.8 J/cm @Temperature 23.0 °C |
0.108 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Rigid Extrusion 87775 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Dart Drop Total Energy | 57.8 J/cm @Temperature 23.0 °C |
0.108 ft-lb/mil @Temperature 73.4 °F |
Procedure B, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Rigid Extrusion 87775 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Dart Drop Total Energy | 57.8 J/cm @Temperature 23.0 °C |
0.108 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
PolyOne Geon™ HTX L1502 Polyvinyl Chloride Alloy (PVC Alloy) Physical properties based on Geon HTX L1502 white 1000.Information provided by PolyOne |
|||
Dart Drop Total Energy | 57.8 J/cm @Temperature 23.0 °C |
0.108 ft-lb/mil @Temperature 73.4 °F |
Procedure B, C.125; ASTM D4226 |
PolyOne Geon™ HTX L1502 Polyvinyl Chloride Alloy (PVC Alloy) Physical properties based on Geon HTX L1502 white 1000.Information provided by PolyOne |
|||
Dart Drop Total Energy | 57.8 J/cm @Temperature 23.0 °C |
0.108 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Dry Blend E6950 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Dart Drop Total Energy | 57.4 J/cm @Temperature 23.0 °C |
0.108 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Dry Blend E7506 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon E7506 is recommended for whites and light pastel colors only. Performs well in extrusion blow molding and high rate fencing capstock applications.Physical properties based on Geon E7506 white 1.. |