Mechanical Properties Metric English Comments
Dart Drop Total Energy 66.7 J/cm

@Temperature 23.0 °C
0.125 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion 87759 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: Finished part testing is required for ASTM E-84 certification. Note: The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by Po..
Dart Drop Total Energy 66.7 J/cm

@Temperature 23.0 °C
0.125 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
PolyOne Geon™ HTX Ultra LA425 Polyvinyl Chloride Alloy (PVC Alloy)
Optimum for Black and Darker Colors below 50L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Ductile/Brittle transition as measured by Instrumented Impact is 5 de..
Dart Drop Total Energy 66.7 J/cm

@Temperature 23.0 °C
0.125 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
PolyOne Geon™ Vinyl Dry Blend E7000 Polyvinyl Chloride, Rigid (PVC, Rigid)
60 degree gloss comparisons: Geon E7000 is 47-49;Geon E7456 is 40-49;Geon E7130 is 38-43;Geon E7370 is 26-31Information provided by PolyOne
Dart Drop Total Energy 66.7 J/cm

@Temperature 23.0 °C
0.125 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
PolyOne Geon™ Vinyl Dry Blend E7001 Polyvinyl Chloride, Rigid (PVC, Rigid)
60 degree gloss comparisons: Geon E7001 is 27-29; Geon E7456 is 40-49; Geon E7130 is 38-43; Geon E7370 is 26-31Information provided by PolyOne
Dart Drop Total Energy 66.7 J/cm

@Temperature 23.0 °C
0.125 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226