Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 35.6 J/cm @Temperature 23.0 °C |
0.0667 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Rigid Extrusion 8700A Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was de.. |
|||
Dart Drop Total Energy | 35.6 J/cm @Temperature 23.0 °C |
0.0667 ft-lb/mil @Temperature 73.4 °F |
Procedure B, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Rigid Extrusion 8700A Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was de.. |
|||
Dart Drop Total Energy | 35.6 J/cm @Temperature 23.0 °C |
0.0667 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Rigid Extrusion L0660 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |