Mechanical Properties Metric English Comments
Modulus of Elasticity 207 GPa

@Temperature -78.0 °C
30000 ksi

@Temperature -108 °F
Haynes Multimet® alloy, 12.7 mm (1/2 in.) thick plate, 1185°C heat treatment, water quenched
Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit..
Modulus of Elasticity 207 GPa

@Temperature 25.0 °C
30000 ksi

@Temperature 77.0 °F
Haynes Hastelloy® C-2000® alloy, flat products
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Modulus of Elasticity 207 GPa

@Temperature 25.0 °C
30000 ksi

@Temperature 77.0 °F
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Modulus of Elasticity 207 GPa

@Temperature 25.0 °C
30000 ksi

@Temperature 77.0 °F
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Modulus of Elasticity 207 GPa

@Temperature 25.0 °C
30000 ksi

@Temperature 77.0 °F
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Modulus of Elasticity 207 GPa

@Temperature 25.0 °C
30000 ksi

@Temperature 77.0 °F
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Modulus of Elasticity 207 GPa

@Temperature 25.0 °C
30000 ksi

@Temperature 77.0 °F
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Modulus of Elasticity 207 GPa

@Temperature 25.0 °C
30000 ksi

@Temperature 77.0 °F
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Modulus of Elasticity 207 GPa

@Temperature 20.0 °C
30000 ksi

@Temperature 68.0 °F
EDRO P1FM #31 Free Machining Holder Steel
EDRO #31 P1-FM is a free machining low alloy steel supplied prehardened to 262-321 HB.P1-FM is characterized by excellent machinability, uniform and consistent hardness in all dimensions, good resis..
Modulus of Elasticity 207 GPa

@Temperature 200 °C
30000 ksi

@Temperature 392 °F
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel
BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303..
Modulus of Elasticity 207 GPa

@Temperature 25.0 °C
30000 ksi

@Temperature 77.0 °F
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C)
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..