Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 207 GPa @Temperature -78.0 °C |
30000 ksi @Temperature -108 °F |
|
Haynes Multimet® alloy, 12.7 mm (1/2 in.) thick plate, 1185°C heat treatment, water quenched Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Modulus of Elasticity | 207 GPa @Temperature 25.0 °C |
30000 ksi @Temperature 77.0 °F |
|
Haynes Hastelloy® C-2000® alloy, flat products Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Modulus of Elasticity | 207 GPa @Temperature 25.0 °C |
30000 ksi @Temperature 77.0 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Modulus of Elasticity | 207 GPa @Temperature 25.0 °C |
30000 ksi @Temperature 77.0 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Modulus of Elasticity | 207 GPa @Temperature 25.0 °C |
30000 ksi @Temperature 77.0 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Modulus of Elasticity | 207 GPa @Temperature 25.0 °C |
30000 ksi @Temperature 77.0 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Modulus of Elasticity | 207 GPa @Temperature 25.0 °C |
30000 ksi @Temperature 77.0 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Modulus of Elasticity | 207 GPa @Temperature 25.0 °C |
30000 ksi @Temperature 77.0 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Modulus of Elasticity | 207 GPa @Temperature 20.0 °C |
30000 ksi @Temperature 68.0 °F |
|
EDRO P1FM #31 Free Machining Holder Steel EDRO #31 P1-FM is a free machining low alloy steel supplied prehardened to 262-321 HB.P1-FM is characterized by excellent machinability, uniform and consistent hardness in all dimensions, good resis.. |
|||
Modulus of Elasticity | 207 GPa @Temperature 200 °C |
30000 ksi @Temperature 392 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |
|||
Modulus of Elasticity | 207 GPa @Temperature 25.0 °C |
30000 ksi @Temperature 77.0 °F |
|
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C) Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |