Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 164 GPa @Temperature 800 °C |
23800 ksi @Temperature 1470 °F |
|
Haynes Waspaloy™ alloy, sheet Age-hardenable superalloy with very good strength at temperatures up 980°C (1800°F), can be cold-formed in the annealed condition, may also be hot formed at 1040°C (1900°F) and above, go.. |
|||
Modulus of Elasticity | 164 GPa @Temperature 100 °C |
23800 ksi @Temperature 212 °F |
Tension |
Schmolz + Bickenbach UGIMA® 316/316L Stainless Steel Bar Description: 316/316L UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 316L, except with respect to machinability. 316/316L UGIM.. |
|||
Modulus of Elasticity | 164 GPa @Temperature 482 °C |
23800 ksi @Temperature 900 °F |
|
Special Metals INCOLOY® 27-7MO Super-Austenitic Stainless Steel INCOLOY® alloy 27-7MO (UNS S31277; EP 1,263,999 B1) is an advanced 7% molybdenum super-austenitic stainless steel offering corrosion resistance in most environments superior to 6% molybdenum super-.. |