Polymer Property : Modulus of Elasticity = 164 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 164 GPa

@Temperature 800 °C
23800 ksi

@Temperature 1470 °F
Haynes Waspaloyâ„¢ alloy, sheet
Age-hardenable superalloy with very good strength at temperatures up 980°C (1800°F), can be cold-formed in the annealed condition, may also be hot formed at 1040°C (1900°F) and above, go..
Modulus of Elasticity 164 GPa

@Temperature 100 °C
23800 ksi

@Temperature 212 °F
Tension
Schmolz + Bickenbach UGIMA® 316/316L Stainless Steel Bar
Description: 316/316L UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 316L, except with respect to machinability. 316/316L UGIM..
Modulus of Elasticity 164 GPa

@Temperature 482 °C
23800 ksi

@Temperature 900 °F
Special Metals INCOLOY® 27-7MO Super-Austenitic Stainless Steel
INCOLOY® alloy 27-7MO (UNS S31277; EP 1,263,999 B1) is an advanced 7% molybdenum super-austenitic stainless steel offering corrosion resistance in most environments superior to 6% molybdenum super-..