Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 158 GPa @Temperature 800 °C |
22900 ksi @Temperature 1470 °F |
|
Haynes Hastelloy® X alloy, sheet Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications includ.. |
|||
Modulus of Elasticity | 158 GPa @Temperature 500 °C |
22900 ksi @Temperature 932 °F |
|
Special Metals INCOLOY® alloy 864 INCOLOY® alloy 8684 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, therma.. |
|||
Modulus of Elasticity | 158 GPa @Temperature 900 °C |
22900 ksi @Temperature 1650 °F |
|
Special Metals INCONEL® alloy 740 Precipitation-Hardenable Ni-Cr-Co Superalloy INCONEL® alloy 740 is a nickel-chromium-cobalt alloy developed by Special Metals Corporation. The alloy is age hardenable by the precipitation of a gamma prime second phase. Potential applicati.. |