Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 92.0 GPa @Temperature 20.0 °C |
>= 13300 ksi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T7 Heat Treatment Condition T7 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Modulus of Elasticity | >= 92.0 GPa @Temperature 20.0 °C |
>= 13300 ksi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Modulus of Elasticity | 92.0 GPa @Temperature 250 °C |
13300 ksi @Temperature 482 °F |
|
CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition AMC225xe is a high quality aerospace grade aluminum alloy (AA2124) reinforced with 25% by volume of ultrafine particles of silicon carbide. It is manufactured by a special powder metallurgy route us.. |