CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition

Category Metal , Metal Matrix Composite , Nonferrous Metal , Aluminum Alloy , 2000 Series Aluminum Alloy
Manufacturer CRP Technology
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AMC225xe is a high quality aerospace grade aluminum alloy (AA2124) reinforced with 25% by volume of ultrafine particles of silicon carbide. It is manufactured by a special powder metallurgy route using a proprietary high-energy mixing process which ensures excellent particle distribution and enhances mechanical properties. The key benefits of AMC225xe for structural applications include: weight saving; increased component stiffness; and high fatigue resistance.The combination of properties achieved with AMC225xe provides the potential for outstanding structural performance in a wide range of markets and applications including:MotorsportPerformance valve trainCylinder linersPistonsConnecting rodsBrake callipersDisk BellsSuspension parts Aerospace & DefenseAero engine vanes Aircraft structureBrakes and WheelsControl SystemsValve BlocksInformation provided by CRP Technology.
Physical Properties Metric English Comments
Density 2.88 g/cc
0.104 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 210
210
HV10
Tensile Strength, Ultimate 65.0 MPa

@Temperature 350 °C
9430 psi

@Temperature 662 °F
short term exposure
194 MPa

@Temperature 260 °C
28100 psi

@Temperature 500 °F
short term exposure
530 MPa

@Temperature 200 °C
76900 psi

@Temperature 392 °F
short term exposure
616 MPa

@Temperature 150 °C
89300 psi

@Temperature 302 °F
short term exposure
650 MPa

@Temperature 20.0 °C
94300 psi

@Temperature 68.0 °F
Tensile Strength, Yield 48.0 MPa

@Temperature 350 °C
6960 psi

@Temperature 662 °F
short term exposure
128 MPa

@Temperature 260 °C
18600 psi

@Temperature 500 °F
short term exposure
448 MPa

@Temperature 200 °C
65000 psi

@Temperature 392 °F
short term exposure
474 MPa

@Temperature 150 °C
68700 psi

@Temperature 302 °F
short term exposure
480 MPa

@Temperature 20.0 °C
69600 psi

@Temperature 68.0 °F
Elongation at Break 5 %
5 %
Modulus of Elasticity 84.0 GPa

@Temperature 300 °C
12200 ksi

@Temperature 572 °F
92.0 GPa

@Temperature 250 °C
13300 ksi

@Temperature 482 °F
102 GPa

@Temperature 200 °C
14800 ksi

@Temperature 392 °F
108 GPa

@Temperature 150 °C
15700 ksi

@Temperature 302 °F
115 GPa

@Temperature 20.0 °C
16700 ksi

@Temperature 68.0 °F
Poissons Ratio 0.30
0.30
Fatigue Strength 305 MPa

@# of Cycles 1.00e+7
44200 psi

@# of Cycles 1.00e+7
R=-1; Kt=1; Rotating Bend
340 MPa

@# of Cycles 1.00e+6
49300 psi

@# of Cycles 1.00e+6
R=-1; Kt=1; Rotating Bend
Thermal Properties Metric English Comments
CTE, linear 13.4 µm/m-°C

@Temperature -75.0 °C
7.44 µin/in-°F

@Temperature -103 °F
14.8 µm/m-°C

@Temperature -25.0 °C
8.22 µin/in-°F

@Temperature -13.0 °F
16.0 µm/m-°C

@Temperature 20.0 °C
8.89 µin/in-°F

@Temperature 68.0 °F
17.6 µm/m-°C

@Temperature 75.0 °C
9.78 µin/in-°F

@Temperature 167 °F
Specific Heat Capacity 0.836 J/g-°C
0.200 BTU/lb-°F
Thermal Conductivity 150 W/m-K
1040 BTU-in/hr-ft²-°F
Melting Point >= 548 °C
>= 1020 °F
Solidus
Solidus 548 °C
1020 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000082 ohm-cm
0.0000082 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 505 °C
941 °F
Solution Heat Treatment