Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.350 GPa @Thickness 0.250 mm, Temperature 23.0 °C |
50.8 ksi @Thickness 0.00984 in, Temperature 73.4 °F |
TD; ASTM D638 |
Mapal Plastics Maplon CFA-HK Polypropylene Sheet Applications: For use with electrical insulation products. For use when flame retardant and static dissipative properties are required. |
|||
Modulus of Elasticity | 0.350 GPa @Thickness 0.430 mm, Temperature 23.0 °C |
50.8 ksi @Thickness 0.0169 in, Temperature 73.4 °F |
ASTM D638 |
Mapal Plastics Maplon CFA-HK Polypropylene Sheet Applications: For use with electrical insulation products. For use when flame retardant and static dissipative properties are required. |