Izod Impact, Notched 4.59 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
8.60 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D-256
Axiall Suprel® SVA 9301 Rigid PVC, Molding
Georgia Gulf Suprel® SVA 9301 is a general purpose injection molding alloy with mid-range properties, providing a balance of impact strength and stiffness and featuring excellent UL flammability li..