Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.51 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
8.45 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID HI5003A PA6/PO, High Impact, High Flow, Good Paintablility Feature: Injection Molding, PA6/PO, High Impact, High Flow, Good PaintablilityApplication: Automotive Exterior PartsCAS No. 25038-54-4, 9010-79-1, 9003-07-0 and 14807-96-6Information provided by LG .. |