Polymer Property : Izod Impact, Notched = 8.37 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.47 J/cm

@Temperature 23.0 °C
8.37 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Cycoloy® CY2000 PC+ABS
Cycoloy resin CY2000 is a flame retardant (FR) PC/ABS blend free from halogen containing FR agents. It was designed to meet CA133 application requirements.This data was supplied by SABIC-IP for the ..