Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.47 J/cm @Temperature 23.0 °C |
8.37 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY2000 PC+ABS Cycoloy resin CY2000 is a flame retardant (FR) PC/ABS blend free from halogen containing FR agents. It was designed to meet CA133 application requirements.This data was supplied by SABIC-IP for the .. |