Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.41 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
8.27 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HI100 ABS, High Impact Feature: Injection Molding, High ImpactApplication: Helmet, Pipe & Fittings, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 4.41 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
>= 8.27 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LUPOY HR5007AE PC/ABS, High Impact Description: Injection Molding, PC/ABS, High Flow, High ImpactApplication: E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 4.41 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
8.27 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical PI641 ABS, High Impact Feature: Extrusion Molding, General Purpose, High ImpactApplication: Pipe FittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 4.41 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
8.27 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.41 J/cm @Thickness 3.17 mm |
8.27 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® ES-0173 ABS, Extrusion Grade Extrusion ABS for the interior of refrigerator with HCFC-141b, down gauging characteristicInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.41 J/cm @Thickness 3.17 mm |
8.27 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GC-0770 H ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.41 J/cm @Thickness 3.17 mm |
8.27 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0852 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.41 J/cm @Thickness 6.35 mm |
8.27 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HP-1011 PC/ABS, Unreinforced Material with superior flowability and small gas generation that can be used in the exterior material of mobile phonesInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.41 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
8.27 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.41 J/cm @Thickness 3.17 mm |
8.27 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® ES-0173 ABS, Extrusion Grade Extrusion ABS for the interior of refrigerator with HCFC-141b, down gauging characteristicInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.41 J/cm @Thickness 3.17 mm |
8.27 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GC-0770 H ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.41 J/cm @Thickness 3.17 mm |
8.27 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0852 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.41 J/cm @Thickness 3.20 mm |
8.27 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron HI40I ABS Injection Molding Grade Automotive applications -Super High Impact , High Rigidity, PaintableInformation provided by Bhansali |
|||
Izod Impact, Notched | 4.41 J/cm @Thickness 6.40 mm |
8.27 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IMC-45M ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |
|||
Izod Impact, Notched | 4.41 J/cm @Thickness 6.40 mm |
8.27 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IMC-45M ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |
|||
Izod Impact, Notched | 4.41 J/cm @Thickness 3.20 mm |
8.27 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron HI40I ABS Injection Molding Grade Automotive applications -Super High Impact , High Rigidity, PaintableInformation provided by Bhansali |
|||
Izod Impact, Notched | 4.41 J/cm @Thickness 6.35 mm |
8.27 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HP-1011 PC/ABS, Unreinforced Material with superior flowability and small gas generation that can be used in the exterior material of mobile phonesInformation provided by Samsung Cheil Industries. |