Polymer Property : Izod Impact, Notched = 8.09 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.32 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
8.09 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Diamond Polymers ABSPC 7430-1005T ABS/PC Injection Molding Grade
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.