Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.90 J/cm @Thickness 4.00 mm, Temperature -20.0 °C |
7.31 ft-lb/in @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PP 1385 PRE-ELEC PP 1385 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Izod Impact, Notched | 3.90 J/cm @Temperature 23.0 °C |
7.31 ft-lb/in @Temperature 73.4 °F |
Practical Use (Water Absorption 3.5%); ASTM-D256 |
Toyobo GLAMIDE® T-803 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 3.90 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
7.31 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers Centrex® 813 General Purpose Injection Molding Grade ASA/AES Centrex 813 resin is a high-gloss, high-impact grade of ASA/AES, a blend of acrylonitrile-styrene-acrylate and acrylonitrile-ethylene-propylene styrene. This injection molding grade with a good bala.. |