Polymer Property : Izod Impact, Notched = 5.80 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 5.80 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
10.9 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87358 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 5.80 J/cm

@Temperature 23.0 °C
10.9 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Asia Pacific)
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..
Izod Impact, Notched 5.80 J/cm

@Temperature 23.0 °C
10.9 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Europe-Africa-Middle East)
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..
Izod Impact, Notched 5.80 J/cm

@Temperature 23.0 °C
10.9 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..