Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.60 J/cm @Temperature 23.0 °C |
10.5 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Europe-Africa-Middle East) High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 5.60 J/cm @Temperature 23.0 °C |
10.5 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East) High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 5.60 J/cm @Temperature 23.0 °C |
10.5 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND PSA 7400 HF PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendHigh impact resistance, high gloss, high heat resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 5.60 J/cm @Thickness 32.0 mm, Temperature 23.0 °C |
10.5 ft-lb/in @Thickness 1.26 in, Temperature 73.4 °F |
ASTM D256 |
Styron Magnum™ 1150 EM Acrylonitrile Butadiene Styrene (ABS) Overview: MAGNUM™ ABS resins are thermoplastic materials which provide an excellent balance to processability, impact resistance and heat resistance as imparted by the various polymer compositions... |