Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.10 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
9.55 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH960 HT10 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platingDrop down resistanc.. |
|||
Izod Impact, Notched | 5.10 J/cm @Temperature -34.0 °C |
9.55 ft-lb/in @Temperature -29.2 °F |
ASTM D256 |
Styron PULSEâ„¢ EXT 200 PC/ABS Engineering Resin Overview: High Heat, High Impact PC/ABS resin for injection molded automotive plating and painting trim applications.Information provided by Styron |