Mechanical Properties Metric English Comments
Izod Impact, Notched 2.549 J/cm

@Thickness 3.20 mm
4.775 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron MIF-35 ABS Injection Molding Grade
High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali
Izod Impact, Notched 2.549 J/cm

@Thickness 3.20 mm
4.775 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron MIF-35 ABS Injection Molding Grade
High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali