Polymer Property : Izod Impact, Notched = 4.4118 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.4118 J/cm

@Thickness 3.20 mm
8.2651 ft-lb/in

@Thickness 0.126 in
ASTM D-256
Bhansali Engineering Abstron SE-32M ABS Sheet Extrusion Grade
Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali
Izod Impact, Notched 4.4118 J/cm

@Thickness 3.20 mm
8.2651 ft-lb/in

@Thickness 0.126 in
ASTM D-256
Bhansali Engineering Abstron HI-34 ABS High Impact Injection Molding
Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali
Izod Impact, Notched 4.4118 J/cm

@Thickness 3.20 mm
8.2651 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron IM-29 ABS Injection Molding Grade
High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali
Izod Impact, Notched 4.4118 J/cm

@Thickness 3.20 mm
8.2651 ft-lb/in

@Thickness 0.126 in
ASTM D-256
Bhansali Engineering Abstron SE-32M ABS Sheet Extrusion Grade
Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali
Izod Impact, Notched 4.4118 J/cm

@Thickness 6.40 mm
8.2651 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron SE-45 ABS Sheet Extrusion Grade
Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali
Izod Impact, Notched 4.4118 J/cm

@Thickness 3.20 mm
8.2651 ft-lb/in

@Thickness 0.126 in
ASTM D-256
Bhansali Engineering Abstron HI-34 ABS High Impact Injection Molding
Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali
Izod Impact, Notched 4.4118 J/cm

@Thickness 3.20 mm
8.2651 ft-lb/in

@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron IM-29 ABS Injection Molding Grade
High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali
Izod Impact, Notched 4.4118 J/cm

@Thickness 6.40 mm
8.2651 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron SE-45 ABS Sheet Extrusion Grade
Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali