Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 4.4079 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.3529 J/cm

@Thickness 6.40 mm
4.4079 ft-lb/in

@Thickness 0.252 in
ASTM D-256
Bhansali Engineering Abstron IM-18 ABS Heat Resistant
High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali
Izod Impact, Notched 2.3529 J/cm

@Thickness 6.40 mm
4.4079 ft-lb/in

@Thickness 0.252 in
ASTM D-256
Bhansali Engineering Abstron IM-18 ABS Heat Resistant
High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali