Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.3529 J/cm @Thickness 6.40 mm |
4.4079 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-18 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.3529 J/cm @Thickness 6.40 mm |
4.4079 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-18 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |