Mechanical Properties Metric English Comments
Izod Impact, Notched 1.91 J/cm

@Temperature -40.0 °C
3.58 ft-lb/in

@Temperature -40.0 °F
ASTM D 256
SABIC Innovative Plastics LNP Verton PV007SV_YW8D151 PA 6
Preliminary data for 35% long fiber single pellet color filled PA6This data was supplied by SABIC-IP for the Americas region.