Izod Impact, Notched 1.471 - 1.56906 J/cm

@Temperature -30.0 - -30.0 °C
2.756 - 2.93950 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 1.52 J/cm Grade Count:1
Overview of materials for PCT, 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr..
Izod Impact, Notched 1.471 - 1.56906 J/cm

@Thickness 3.17 - 6.35 mm
2.756 - 2.93950 ft-lb/in

@Thickness 0.125 - 0.250 in
Average value: 1.52 J/cm Grade Count:1
Overview of materials for PCT, 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr..