Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.471 - 1.56906 J/cm @Temperature -30.0 - -30.0 °C |
2.756 - 2.93950 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 1.52 J/cm Grade Count:1 |
Overview of materials for PCT, 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr.. |
|||
Izod Impact, Notched | 1.471 - 1.56906 J/cm @Thickness 3.17 - 6.35 mm |
2.756 - 2.93950 ft-lb/in @Thickness 0.125 - 0.250 in |
Average value: 1.52 J/cm Grade Count:1 |
Overview of materials for PCT, 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr.. |