Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.37 J/cm @Temperature -30.0 °C |
4.44 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Izod Impact, Notched | 2.37 J/cm @Temperature -30.0 °C |
4.44 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Asia Pacific) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Izod Impact, Notched | 2.37 J/cm @Temperature -30.0 °C |
4.44 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Europe-Africa-Middle East) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |