Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 10.3 J/cm @Thickness 3.17 mm |
19.3 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||