Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Extruded
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 4.3 g/10 min

@Load 10.0 kg,
Temperature 220 °C
4.3 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.1 MPa
6680 psi
5 mm/min; ASTM D638
Elongation at Break 35 %
35 %
5 mm/min; ASTM D638
Flexural Strength 56.9 MPa
8250 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.11 GPa
306 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 2.94 J/cm

@Thickness 6.35 mm
5.51 ft-lb/in

@Thickness 0.250 in
ASTM D256
10.3 J/cm

@Thickness 3.17 mm
19.3 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C

@Thickness 6.40 mm
196 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 100 °C
212 °F
B/50; ISO R306