Izod Impact, Notched 13.4 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
25.1 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Axiall 9190 Rigid PVC, Molding
Georgia Gulf 9190 was developed to aid compliance with source reduction initiatives especially when low temperature impact strength is a concern. It has superior properties, which in most cases wil..