Mechanical Properties Metric English Comments
Izod Impact, Notched 6.67 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
12.5 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Axiall 8132 Rigid PVC, Extrusion
Georgia Gulf 8132 is a rigid PVC compound designed for applications where transparency is important. This product remains unchanged except for the coded name and was previously identified as 3132. ..