Mechanical Properties Metric English Comments
Izod Impact, Notched 4.27 - 5.87 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
8.00 - 11.0 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D-256
Axiall Suprel® SVA 9812 Rigid PVC, Extrusion
Georgia Gulf Suprel® SVA 9812 Alloy is an extrusion grade thermoplastic designed for sheet or profile applications requiring high impact resistance. Key features of Suprel 9812 alloy are flame ret..