Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 10.7 J/cm @Thickness 3.17 mm |
20.0 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 9202J Rigid PVC, Molding Georgia Gulf 9202J is suitable for all types of food packaging. The compound provides low taste and odor properties and contains an ultraviolet light stabilizer which protects light sensitive produ.. |
|||
Izod Impact, Notched | 10.7 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
20.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall SP-6235 Rigid PVC, Molding Georgia Gulf SP-6235 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, high melt flow and exceptionall.. |